http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018162529-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C70-10 |
filingDate | 2017-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f27879b3f270c1f0790ae3862d0685fc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_caf54ab304b2118371c425e3459a239f |
publicationDate | 2018-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018162529-A |
titleOfInvention | Totally aromatic polyamide profile fiber |
abstract | PROBLEM TO BE SOLVED: To provide a wholly aromatic polyamide fiber excellent in adhesiveness with a resin or the like in addition to high strength. SOLUTION: An all-aromatic polyamide modified cross-section fiber having a single fiber cross-section having recesses and the number of which is 2 or more and 15 or less. Furthermore, the strength of the fiber is in the range of 15 to 30 cN / dtex, the wholly aromatic polyamide fiber is a para-type wholly aromatic polyamide fiber, and further made of a copolymerized aromatic polyamide resin. preferable. Or the fiber reinforced resin composite which consists of said wholly aromatic polyamide modified cross-section fiber and resin. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7148350-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020059931-A |
priorityDate | 2017-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.