http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018145360-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L93-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L57-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-02 |
filingDate | 2017-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45fead10994bc853c2f4b821abd12cde |
publicationDate | 2018-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018145360-A |
titleOfInvention | Bale moldings of conjugated diene polymers |
abstract | The present invention provides a bale-molded product of a conjugated diene polymer that can suppress peeling of the conjugated diene polymer particles from the surface and has a reduced expansion coefficient. SOLUTION: A conjugated diene, preferably 1,3-butadiene, 100 parts by mass of an isoprene-based polymer and an SP value of 7 to 9.5 [(cal / ml) 1/2 ], preferably a petroleum resin, A bale molded article of a conjugated diene polymer containing 3 to 60 parts by mass of an additive which is a malon indene resin, a terpene resin, or a rosin resin. It is preferable that the additive has a softening point of -40 to 100 ° C. The molded article, wherein the conjugated diene copolymer contains 30 to 90% by mass of a conjugated diene polymer having a molecular weight of 1,000,000 or more. [Selection] Figure 3 |