http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018124460-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c97f90ab12b35b650d5fd039ed7a41a5 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08795 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08711 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08755 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2017-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dff1a31c6abeece13bb9688a74f39a7a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fac8401453c67de6143a5b0eb962da8c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d46cce1c86626eb0e55c3d967fc0b8e2 |
publicationDate | 2018-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018124460-A |
titleOfInvention | Toner for electrostatic image development |
abstract | An object of the present invention is to provide a toner for developing an electrostatic image capable of suppressing the occurrence of gloss memory while being excellent in low-temperature fixability and heat-resistant storage stability. The toner for developing an electrostatic charge image of the present invention contains an amorphous polyester resin, a crystalline polyester resin, and a styrene / acrylic resin, and also contains a release agent, and the amorphous polyester resin and the crystal. The proportion of the crystalline polyester resin in the total amount of the conductive polyester resin is more than 40% by mass to 60% by mass, and the storage elastic modulus G ′ before being left to stand at the temperature X ° C. is 1.0 × 10 8 Pa. The value of the ratio of the storage elastic modulus G ′ after thermal storage at a temperature X ° C. after standing at a temperature X ° C. for 2 hours with respect to the storage elastic modulus G ′ before thermal storage at a temperature X ° C. The storage elastic modulus G ′ after thermal standing at a temperature X ′ ° C. when the maximum value is is 1.0 × 10 8 to 5.0 × 10 8 Pa. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018173500-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020106685-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017211648-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017211647-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020003739-A1 |
priorityDate | 2017-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 134.