http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018058915-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3fedd1aa5fe3bde139f0fbf7bd16550b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-00 |
filingDate | 2016-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e2a8abd39cce9a429915f947ac5c3a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4679aa66e6a1a9b68580052af08e719f |
publicationDate | 2018-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018058915-A |
titleOfInvention | Adhesive composition |
abstract | The present invention provides a pressure-sensitive adhesive composition having excellent ultraviolet absorption performance, little change in appearance during use, and excellent reworkability when peeled. (A) an acrylic polymer in which the proportion of monomers having an amide group in the monomer composition is 1 to 25% by weight, (b) a compound having a triazine structure, and (c) a compound having a benzotriazole structure The pressure-sensitive adhesive composition is characterized in that the total of the component (b) and the component (c) is 10 to 40 parts by weight with respect to 100 parts by weight of the component (a). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7306560-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019189030-A1 |
priorityDate | 2016-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 134.