http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018056425-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-38 |
filingDate | 2016-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee94a3851f062d15534a3ac4295b4c6e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d8d5ca4384fabc9323e284fe97fe20f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9a78877fb9076846bebe130ff339d33 |
publicationDate | 2018-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018056425-A |
titleOfInvention | Non-aqueous lithium storage element |
abstract | The present invention provides a non-aqueous lithium storage element having high peel strength of a positive electrode, high energy density, high input / output characteristics, and excellent high load charge / discharge cycle durability. A non-aqueous lithium storage element including a positive electrode, a negative electrode, a separator, and a non-aqueous electrolyte containing lithium ions, wherein the positive electrode includes a positive electrode current collector and the positive electrode current collector. A positive electrode active material layer on one or both sides, the positive electrode active material layer contains a positive electrode active material containing a carbon material and a binder, the negative electrode comprises a negative electrode current collector, and the negative electrode A negative electrode active material layer on one or both sides of the current collector, the negative electrode active material layer contains a negative electrode active material capable of occluding and releasing lithium ions, and the positive electrode is a total mass of the positive electrode active material layer In the differential scanning calorimetry of the positive electrode active material layer, the melting start temperature of the binder is 25 ° C. or more and 250. Non-aqueous lithium type not detected in the temperature range below ℃ Electric element. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200039742-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111095650-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111095650-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2020017515-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020017515-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115763703-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102366885-B1 |
priorityDate | 2016-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 102.