http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018053013-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-16 |
filingDate | 2016-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e33a69b33ec409d327c98245f11517b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0345640b0a176e969bea08b2181304ef |
publicationDate | 2018-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018053013-A |
titleOfInvention | Resin composition and film comprising resin composition |
abstract | An object of the present invention is to provide a resin composition which is excellent in transparency and tear resistance and hardly changes in physical properties at storage temperature, and is excellent in transparency and tear resistance and at storage temperature. The object is to provide a film whose physical properties are not easily altered. A resin composition containing 61 to 90% by mass of an acrylic resin (A) and 10 to 39% by mass of a vinylidene fluoride resin (B), which is 10 ° C. from 30 ° C. to 200 ° C. by a differential scanning calorimeter. The crystal melting enthalpy observed in the process of raising the temperature at 0 / min is 0 to 5 J / g, and the acrylic resin (A) contains a resin having a core-shell structure in which an acrylic rubber is used as a core and a graft portion is provided. , Resin composition. [Selection figure] None |