http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018043448-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1837840b0d7f1d216335a0331a4bd15a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2016-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9babfe605e90f7b7e4ef3dd41d13df50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b33dd4f320cf4ccaf21a6cbf0890a363 |
publicationDate | 2018-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018043448-A |
titleOfInvention | Laminated polyester film |
abstract | A laminated polyester film having a cured layer capable of preventing bleeding of a polyester oligomer when heated at a high temperature for a long time. A polyfunctional aziridine compound (a1) having at least three aziridinyl groups in the molecule and having an aziridinyl group content of 1 to 15 mmol / g, an aziridinyl group ring-opening catalyst (a2), ammonia and A cured layer (A) of an oligomer bleed inhibitor (A ′) containing amines (a3) is laminated on the polyester film (B) and has an initial haze value (Ha) of 150 ° C. A laminated polyester film having a change amount (ΔH) of 1% or less from the haze value (Hb) after heating for 3 hours. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200125474-A |
priorityDate | 2016-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 166.