http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018039929-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a011a6e6ab11a97077c41da9d26881b6 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 |
filingDate | 2016-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_856aaa62dc8d3a643da3645886c16549 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_edefae4da80da4e66de679cf078c73b5 |
publicationDate | 2018-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018039929-A |
titleOfInvention | Aqueous liquid absorbent resin particles, and absorbent body and absorbent article using the same |
abstract | The present invention provides a method for producing aqueous liquid-absorbent resin particles capable of satisfying both liquid permeability between swollen gels and absorption performance under a load even after transport and diaper production steps. A water-soluble vinyl monomer (a1) and / or a hydrolyzable vinyl monomer (a2) and a cross-linked polymer (A) having a cross-linking agent (b) as essential constituent units, and a polyvalent having 4 or less carbon atoms. The alcohol (c) contains a polyvalent metal salt (d), and the weight ratio (c) / (d) of the polyhydric alcohol (c) to the polyvalent metal salt (d) is 0.95 to 5.5. An aqueous liquid absorbent resin particle having a surface coverage of 50 to 100% with a polyvalent metal salt (d) obtained by elemental mapping using energy dispersive X-ray analysis. [Selection figure] None |
priorityDate | 2016-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |