http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018031094-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-263 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-155 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-4209 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-407 |
filingDate | 2016-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc34c4dbf527c39ff407a60a3fbb6c9a |
publicationDate | 2018-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018031094-A |
titleOfInvention | Fiber structure and manufacturing method thereof |
abstract | The present invention provides a fiber structure excellent in moisture absorption / release properties and initial moisture absorption rate, and preferably excellent in rigidity when wet, and a method for producing the same. The difference (R2−R1) between the moisture absorption rate R1 (%) at a temperature of 20 ° C. and a humidity of 40% RH and the moisture absorption rate R2 (%) at a temperature of 20 ° C. and a humidity of 90% RH is 40% or more. In addition, after adsorbing a hygroscopic polymer having an absorption rate of 10 times or more of distilled water and a metal halide salt to the fiber structure, an adsorbent for exchanging humidity is obtained as necessary. [Selection] Figure 1 |
priorityDate | 2016-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |