abstract |
[PROBLEMS] To provide a molding material with excellent retention stability capable of producing a molded product with excellent moldability, mechanical properties, and water resistance. A molding material containing a urea-modified polyolefin (a), a polypropylene resin (b), a reinforcing fiber (c), and a terpene resin (d), which is contained in a matrix resin component in the molding material. The group content is 0.0005 to 140 mmol with respect to 100 g of the matrix resin component, and the reinforcing fiber (c) is sizing-treated with the polyfunctional compound (s), and the components (c) and (d) ) Is bonded with a polypropylene resin component comprising components (a) and (b), the component (d) has an SP value of 6.5 to 9, and the component (s) The molding material characterized by being lower than the SP value of [Selection figure] None |