http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018009103-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fb2edb0f237a90d982f2dce09ad61976 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-00 |
filingDate | 2016-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c148210a48714201e6f8756c06eff989 |
publicationDate | 2018-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018009103-A |
titleOfInvention | Method for producing polyurethane foam |
abstract | Disclosed is a method for producing a polyurethane foam having improved physical properties by improving the poor compatibility between an HFO foaming agent and a polyester polyol. A method for producing a polyurethane foam using at least a polyisocyanate, a polyol, a hydrofluoroolefin-based blowing agent, a catalyst, and a surfactant, wherein the polyester polyol (A) used as a part of the polyol is an alcohol. The manufacturing method of the polyurethane foam which uses 10 weight% or more of polyethyleneglycol and / or polypropylene glycol of number average molecular weight 200-2000 as a component with respect to 100 weight% of all the alcohol components in a polyester polyol (A). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7088763-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020012027-A |
priorityDate | 2016-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.