http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017511425-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-28 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-16 |
filingDate | 2015-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017511425-A |
titleOfInvention | Method for producing polyamide |
abstract | The process produces a polyamide having an extracted fraction of 2-10% oligomers. The method includes the steps of introducing a monomer into the reactor and polymerizing the reactor monomer to form a first intermediate having an oligomeric fraction of greater than 10%, the oligomer repeating unit having 2 to 20 oligomers A step of being a compound having The method comprises the steps of transferring a first intermediate from a reactor to an extractor; and introducing a water into the extractor and a second intermediate having an oligomeric extract fraction that is smaller than the oligomer extract fraction of the first intermediate Wherein water is introduced at a temperature of less than 100 ° C., and the water comprises a step in which 0.1 to 0.3% by weight of plasticizer is included when introduced into the extractor. Further, the method includes transferring the second intermediate from the reactor to a dryer and sending air at a temperature below 125 ° C. [Selection] Figure 1 |
priorityDate | 2014-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |