http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017217598-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3fbd7cacf2a93bef7f4f68e21602f601 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 |
filingDate | 2016-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58bc62e8f7a1554c45aa50c944a38669 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c46a5310e85b0cc706d33cd7c5b1ae71 |
publicationDate | 2017-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017217598-A |
titleOfInvention | Film formation method |
abstract | In a method for forming a coating on a lightweight inorganic substrate, a coating excellent in substrate reinforcement, adhesion, durability and the like is efficiently obtained. A lightweight inorganic base material having a bulk density of 0.8 g / cm3 or less includes an epoxy resin, an amine curing agent, and a nonaqueous solvent as a first film forming material, and the ratio of the nonaqueous solvent is as described above. 40 to 400 parts by weight based on 100 parts by weight of the total solid content of the epoxy resin and the amine curing agent, and the non-aqueous solvent is selected from an aliphatic hydrocarbon solvent, a hydroxyl group, an ether group, and an ester group The thing containing the polar solvent with a boiling point of 100-260 degreeC which has a polar group more than a seed | species is used. [Selection figure] None |