http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017200773-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0f705f295f4ba571f5311e5ef1b57807 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 |
filingDate | 2017-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05f61db408a7c8be34e4c225f0996a93 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29c73727f3e84d3efac3560d35e5b9d2 |
publicationDate | 2017-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017200773-A |
titleOfInvention | Decorative plate and its construction method |
abstract | Provided is a decorative board in which the function of the photocatalyst is not deteriorated even when a protective film attached to the surface of the decorative board carrying the photocatalyst is peeled off. A decorative plate in which a photocatalyst made of titania is supported on a base material, wherein a protective film is laminated on the photocatalyst via an acrylic adhesive so as to be peeled off. Decorative board. [Selection] Figure 1 |
priorityDate | 2015-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |