http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017165841-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a7b097bfd3f350ed27ffa53e1f114d1a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3477 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 |
filingDate | 2016-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f864795dda12d90d793b338352f51e3 |
publicationDate | 2017-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017165841-A |
titleOfInvention | Material for medical device member and method for manufacturing medical device member |
abstract | The material of a medical device member can improve perforation strength. A material for a medical device member includes a fluorine elastomer as a main component and a crosslinking agent that crosslinks the molecules of the fluorine elastomer, and the crosslinking agent has a first half-life temperature of 1 minute. A first organic peroxide that is a temperature; and a second organic peroxide that is a second temperature having a one-minute half-life temperature of 20 ° C. or more higher than the first temperature. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020045397-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7193705-B2 |
priorityDate | 2016-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.