http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017165628-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_66828b5658002eedf4c25aec4b47c898 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 |
filingDate | 2016-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2aac19a754c3ac1bbabde4ec0751003e |
publicationDate | 2017-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017165628-A |
titleOfInvention | Fast-setting grout composition |
abstract | [Problem] To provide a fast-hardening grout composition capable of imparting good initial strength development properties while ensuring a predetermined pot life even in a high-temperature environment such as summer. A cement, calcium aluminate, gypsum, a set retarder, a thickener, a water reducing agent, and an aggregate, and 100 parts by mass of the binder containing the cement, calcium aluminate, and gypsum. The thickener content is 0.01 to 0.1 parts by mass, the setting retarder content is 0.3 to 1.5 parts by mass, and the aggregate content is 105 to 175 parts by mass. Quick-hardening grout composition characterized by the above. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020083698-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7125335-B2 |
priorityDate | 2016-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.