http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017162755-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 |
filingDate | 2016-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86020d7c9b18ac9698674c35eb1d06d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3849ed48f7b10501b719561386a43ff |
publicationDate | 2017-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017162755-A |
titleOfInvention | Separator |
abstract | PROBLEM TO BE SOLVED: To provide a separator having a high melting point and strength and capable of being thinned and having a low molecular weight component and excellent cleanliness. SOLUTION: For 100 parts by weight of ultrahigh molecular weight polyethylene having an intrinsic viscosity ([η]) of 10 dl / g or more and 80 dl / g or less, a weight average molecular weight (Mw) of 600,000 or less and a melt tension at 210 ° C. of 100 mN or more. And a separator made of an ultrahigh molecular weight polyethylene composition having strain hardenability and containing 5 to 5000 parts by weight of polyethylene having a density according to JIS K6760 of 935 kg / m 3 or more and 960 kg / m 3 or less. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113285184-A |
priorityDate | 2016-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links