http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017154324-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c94d5b30306331580c7e070b5d44327e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 2016-02-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53aff9b766c1d347f086efa9b691c652 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e6d485b2f7e16e060ae1997da997794 |
publicationDate | 2017-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017154324-A |
titleOfInvention | Design metal plate and manufacturing method thereof |
abstract | [PROBLEMS] To suppress deterioration of a design applied to a design film during the production of the design metal plate, and to maintain the adhesion between the design film and the metal plate even under a severe environment of high temperature and high humidity. Provided are a new and improved design metal plate having a high organic solvent resistance and a method for producing the same. In order to solve the above problems, according to one aspect of the present invention, a metal plate, a lower layer side adhesive layer laminated on the metal plate, and an upper layer side adhesive layer laminated on the lower layer side adhesive layer are provided. A design film laminated on the upper layer side adhesive layer, the lower layer side adhesive layer includes a lower layer side adhesive, the upper layer side adhesive layer includes an upper layer side adhesive and hydrophobic silica fine particles, The softening temperature of the upper layer side adhesive is 80 ° C. or lower, the softening temperature of the lower layer side adhesive is 90 ° C. or higher, and the upper layer side adhesive layer contains 1 hydrophobic silica fine particle per 100 parts by mass of the upper layer side adhesive. The design metal plate characterized by including -10 mass parts is provided. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107216843-A |
priorityDate | 2016-02-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 169.