http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017136805-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B17-10 |
filingDate | 2016-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81deb314371f9777c1edc6f702fc3ea8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78d9904e5a039b72815cbb9023b8a832 |
publicationDate | 2017-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017136805-A |
titleOfInvention | Laminate |
abstract | [Problem] To provide a laminate having excellent handling properties and exhibiting excellent safety performance when used as an interlayer film for safety laminated glass, and moreover, the handling properties are less likely to deteriorate when the laminate is stored for a long period of time. Offer. The present invention includes a layer (1) and a layer (2) on at least one side of the layer (1), at least one of the outermost layers being the layer (1), and a laminated structure of three or more layers The layer (1) contains the thermoplastic resin (I), the layer (2) contains the thermoplastic resin (II), and 100 parts by mass of the thermoplastic resin (II). A laminate comprising 4 to 200 parts by mass of the plasticizer A, and HV (A) ≧ 30 when the hydroxyl value of the plasticizer A is HV (A) mgKOH / g. [Selection figure] None |