http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017132978-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4283a2f8ade5dc582d75300427a38e50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-50 |
filingDate | 2016-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b8cef044593019e6c7f29771cadf8a6 |
publicationDate | 2017-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017132978-A |
titleOfInvention | Method for producing homogenized synthetic rubber |
abstract | Provided is a production method for quickly and easily obtaining a synthetic rubber having a low degree of dispersion regardless of the molecular weight. (2) A method for producing a homogenized synthetic rubber, comprising a step of subjecting synthetic rubber to a high-speed jet treatment and / or a high-speed flow treatment. Prior to step (2), the above production method further comprises (1) a step of synthesizing a synthetic rubber. The synthetic rubber is a (meth) acrylic acid ester polymer, the weight average molecular weight of the homogenized synthetic rubber is 100,000 to 1,000,000, and the ratio of the weight average molecular weight to the number average molecular weight is 2 Said manufacturing method which is .5 or less. [Selection figure] None |