Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_887e125008cf84c53554d9e68cf7f02b |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2363-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-686 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-24 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-66 |
filingDate |
2016-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce7dd356aacbb581762c9be0c555dbfd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3e5a9632374633e6b5bce2380564549 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e1564eea4800ab171c2b129b30f2e6c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8b0503e827a574293799e4fe045c2da http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fee9fc386f8dfcae2f0544ffd6305461 |
publicationDate |
2017-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2017125179-A |
titleOfInvention |
Fast-curing thiol epoxy resin with improved compressive strength performance |
abstract |
The present invention relates to an epoxy resin and a method for forming an epoxy resin. A resin comprising a reaction product of one or more polythiols, one or more polyepoxides, one or more fillers, and one or more amine catalysts. A resin wherein the polythiol has between 2 and about 10 thiol moieties and the polyepoxide has between 2 and about 10 epoxy moieties. One or more amine catalysts represented by the chemical formula (NR1R2R3). (R1 to R3 are each independently a linear / branched C1-20 alkyl or two or more of R1 to R3 are combined to form a cycloalkyl) Compressive strength of at least 14 ksi at 2% offset at 70 ° F, And a compressive strength of at least 8 ksi with a 2% offset at 190 ° F. [Selection figure] None |
priorityDate |
2015-11-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |