http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017114968-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 |
filingDate | 2015-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df71f7bcc9f8b0a73d515ff6c550aa7a |
publicationDate | 2017-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017114968-A |
titleOfInvention | Polyarylene sulfide resin composition, molded article and production method |
abstract | PROBLEM TO BE SOLVED: To provide a polyarylene sulfide resin composition in which variation in conductivity in the surface and thickness direction is suppressed and imparted uniform and sufficient conductivity, a molded product formed by molding the resin composition, and the polyarylene sulfide To provide a method for producing a resin composition. SOLUTION: A polyarylene sulfide resin (A) having a melt viscosity (V6) measured at 300 ° C. in the range of 5 to 1000 [Pa · s] and an ionic liquid (B) are blended as essential components. A polyarylene sulfide resin composition, a molded product obtained by molding the polyarylene sulfide resin composition, the polyarylene sulfide resin (A), and an ionic liquid (B). A method for producing a polyarylene sulfide resin composition, characterized by melting and kneading at a melting point or higher of the polyarylene sulfide resin (A) as an essential component. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11274207-B2 |
priorityDate | 2015-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 149.