http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017111460-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-125 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1355 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-132 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-135 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-081 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-12 |
filingDate | 2017-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b61a4089da426755dfebf75503676ae3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2224584a4eca145c36eaa6312225be9e |
publicationDate | 2017-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017111460-A |
titleOfInvention | Liquid developer |
abstract | The present invention relates to a liquid developer that does not affect a printing apparatus even during long-time operation, and a method for manufacturing the same. A liquid developer in which toner particles containing a polyester-containing resin and a pigment are dispersed in an insulating liquid in the presence of a dispersant, and the insulating liquid is held at 40 ° C. for 30 minutes. And a liquid developer in which toner particles containing a liquid developer, a resin containing polyester, and a pigment are dispersed in an insulating liquid in the presence of a dispersant, wherein the volatilization rate of the liquid developer is less than 0.26% by mass, Step 1: Melting and kneading resin and pigment containing polyester and pulverizing to obtain toner particles, Step 2: Adding a dispersant to the toner particles obtained in Step 1 and dispersing them in an insulating liquid. A step of obtaining a dispersion, and a step 3: wet pulverizing the toner particle dispersion obtained in step 2 to obtain a liquid developer, wherein the insulating liquid has a volatility after holding at 40 ° C. for 30 minutes. Production of liquid developer that is less than 0.26% by mass Method. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019177136-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019159241-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11624987-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7057177-B2 |
priorityDate | 2015-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 72.