http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017105878-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2015-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e92401d07c4a7c0cd666a2524a4e4b0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_189d213448adcea6c0576929cab6da0f |
publicationDate | 2017-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017105878-A |
titleOfInvention | Adhesive tape and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide an adhesive tape having excellent adhesive strength and in which the entire adhesive tape is not easily deformed by an external force. The present invention is an adhesive tape having an adhesive layer (B) on at least one surface side of a base material (A), and has a storage elastic modulus measured at a temperature of 20 ° C. and a frequency of 10.0 Hz. (E'20) is 1.0 × 107 Pa or more, the storage elastic modulus (E'60) measured at a temperature of 60 ° C. and a frequency of 10.0 Hz is 1.0 × 106 Pa or more, and the substrate. Adhesive tape in which the ratio of the thickness of the pressure-sensitive adhesive layer (B) to the thickness of (A) [thickness of the pressure-sensitive adhesive layer (B) / thickness of the base material (A)] is 1/100 to 30/100. To solve the above-mentioned problems. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019244652-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022230622-A1 |
priorityDate | 2015-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 184.