Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-1515 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 |
filingDate |
2016-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8034eb37186a14166a78f29ddac20a1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e09a7f7ec696edeaca7685b0ebaa3361 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_691c2c7dd4493d74565c914dbdac1d7d |
publicationDate |
2017-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2017095671-A |
titleOfInvention |
Molded article and polyamide resin composition |
abstract |
[PROBLEMS] To provide a molded article excellent in heat aging resistance, calcium chloride resistance and surface appearance. A molded article having a thickness of 0.56 mm or more obtained by molding a polyamide resin composition, which is obtained by Fourier transform infrared spectroscopic analysis after heat treatment in air at 150 ° C. for 1000 hours. A molded article in which the ratio (Y / Z) of the peak intensity Y of the carboxyl group on the surface of the article to the peak intensity Z of the carboxyl group at a depth of 0.28 mm from the surface of the article is 5.0 or less. [Selection] Figure 3 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019081895-A |
priorityDate |
2015-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |