http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017075209-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ebdfc88803aa0e0bb776ddb9db35fda |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate | 2015-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8605a359a6c24b98cf0636e36245a51f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a4d91f356caa520f5b9e594573c4d4d |
publicationDate | 2017-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017075209-A |
titleOfInvention | POLYPROPYLENE RESIN COMPOSITION, MATERIAL MATERIAL USING SAME, AND MOLDED BODY USING SAME |
abstract | PROBLEM TO BE SOLVED: To provide a polypropylene resin composition excellent in moldability and excellent in rigidity (flexural modulus), impact property and transparency, a raw material made from the raw material, and a molded body made from the raw material. A polypropylene resin composition containing 55 to 85% by weight of component A satisfying conditions a1 to a3 and 15 to 45% by weight of component B satisfying condition b. (A and B total 100% by weight) a1: Component A contains propylene homopolymer (A1) 40 to 90% by weight and propylene-α-olefin random copolymer (A2) 10 to 60% by weight ( (The sum of (A1) and (A2) is 100% by weight), a2: MFR of component A as a whole (230 ° C., 2.16 kg load) is 0.5 to 200 g / 10 min, a3: component A is 110 Melting peak temperature (Tm) in the range of ˜170 ° C. (DSC method) b: Component B is at least one elastomer. [Selection figure] None |
priorityDate | 2015-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |