http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017064707-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_32681f1832d227fe8df23d12a37f67a8
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0244
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-063
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D1-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-025
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00
filingDate 2016-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ee4e18fba0e0c89b2c418a2a84cfae6
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b94322afa3410deff00e672bffb9113
publicationDate 2017-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2017064707-A
titleOfInvention Photocatalyst paint
abstract Provided is a photocatalyst-coated body capable of realizing sufficient photocatalytic activity and adhesion to a base material without greatly impairing the appearance of the base material, particularly exterior building materials. The structure includes a base material, an intermediate layer provided on the base material, and a photocatalyst layer provided on the intermediate layer. The intermediate layer includes inorganic oxide particles having an average particle size of nano-size, and the photocatalyst layer includes photocatalyst particles having an average particle size of more than 0 μm and less than 10 μm, and inorganic oxide particles having an average particle size of nano-size. Comprising. The sum of the film thickness of the intermediate layer and the photocatalyst layer is 0.3 μm or more and 1.5 μm or less. [Selection figure] None
priorityDate 2015-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1135851-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013008718-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000014755-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010172797-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID4139
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419476681

Total number of triples: 30.