Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c389d310f52125a947b3408cb0cf3283 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2315-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-322 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2307-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-212 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-16 |
filingDate |
2015-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_618012d35797daa4c51d62f1d73876d5 |
publicationDate |
2017-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2017039881-A |
titleOfInvention |
Rubber wet masterbatch manufacturing method, rubber composition manufacturing method, and tire manufacturing method |
abstract |
To provide a method for producing a rubber wet masterbatch, which is a raw material of vulcanized rubber having excellent fatigue properties, low heat build-up properties and tensile properties. A rubber wet masterbatch is produced by a method including a step of preparing a latex having a magnesium content of 150 ppm or less, a step of producing a mixed solution, and a step of causing coagulation of the mixed solution to obtain a coagulated product. The latex includes rubber particles having a 90% by volume particle size of 2 μm or less. The step of producing a mixed liquid includes a step of mixing the latex and the dispersion solvent. The step of producing a mixed solution further includes a step of mixing the slurry containing the filler and the latex solution obtained by mixing the latex and the dispersion solvent. The step of obtaining the coagulum includes a step of separating the coagulum and the waste liquid. The method for producing the rubber wet masterbatch satisfies the following formula I. a / b ≧ 65 (Formula I) (In Formula I, a represents the COD value (mg / L) of the waste liquid. b represents the rubber content (mass%) in the mixed solution.) Figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019112545-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019112542-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7067917-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019130800-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019058807-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7066398-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7163924-B2 |
priorityDate |
2015-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |