http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017030261-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-02 |
filingDate | 2015-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0d4d61c0fc04ec001512ff0a4bed2669 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f013458a92079aa3c7b57025884c82d |
publicationDate | 2017-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017030261-A |
titleOfInvention | Laminate |
abstract | Provided is a laminate formed by an extrusion laminating method, which has a good surface slip property and anti-blocking property and does not require powder spraying on the surface after extrusion lamination molding. SOLUTION: The outermost layer includes at least an outermost layer and a base material layer, and the outermost layer is composed of an olefin resin composition (A) containing 0.01 to 50% by weight of inorganic fine particles or organic fine particles, and has a height of 0 on the surface. A laminate having 10 or more projections of 5 μm or more per square mm. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020040361-A |
priorityDate | 2015-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 44.