http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017007886-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d97cb748898aa080b013f7f35bc8b434 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-50 |
filingDate | 2015-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1bd455f1b53f198368806e6fd44acc47 |
publicationDate | 2017-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017007886-A |
titleOfInvention | Method for producing magnesium hydroxide slurry and magnesium hydroxide slurry |
abstract | A method for producing a magnesium hydroxide slurry capable of sufficiently suppressing gelation and hardening of a magnesium hydroxide slurry, and a magnesium hydroxide slurry for removing sulfur oxides in flue gas obtained by the production method. SOLUTION: Naphthalenesulfonic acid formaldehyde condensate or a salt thereof is added in a step of adding magnesium to lightly burned magnesium oxide having an average particle size of 10 μm or less to cause hydration to produce magnesium hydroxide. A method for producing a magnesium hydroxide slurry. [Selection figure] None |
priorityDate | 2015-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |