Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2998 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00801 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00491 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-0065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00637 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-0058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-27 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F257-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-2641 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-2676 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F257-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 |
filingDate |
2014-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2016-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2016507623-A |
titleOfInvention |
Hybrid latex containing polymer particles having a core-shell structure and method for producing the same |
abstract |
The present invention is a hybrid latex comprising polymer particles having a core-shell structure, wherein (1) the comonomer of the core comprises (a) a monovinyl aromatic compound and (b) an unsaturated carboxylic acid ester; ) The comonomer of the shell comprises (a) a monovinyl aromatic compound and (b) a conjugated diene; the glass transition temperature of the core is in the range of −50 ° C. to 50 ° C., and the glass transition temperature of the shell is − The hybrid latex is in the range of 50 ° C to 50 ° C. The present invention also relates to the use of the hybrid latex in a polymer-based waterproofing material and a polymer cement mortar. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020045515-A1 |
priorityDate |
2013-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |