http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016206632-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b9a255559e1d94f20510a17a673b1078 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-0821 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08711 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08795 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G15-0865 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2015-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68b47da2d8676356efbf71541dc279c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9dc4f1834facaeac5d541899068ca55a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a5f8a16860508ad9e79f26ac64335975 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4b7ff899c852156403f5a0ee42ef43d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b54aab98e63341e891029fd810dcfa7b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_211300d4b605ec96b823b7712d080f08 |
publicationDate | 2016-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016206632-A |
titleOfInvention | Toner, developer, image forming apparatus and developer accommodating unit |
abstract | Provided is a toner having good low-temperature fixability, heat-resistant storage stability, and stress resistance. In a X-ray diffraction measurement, a diffraction peak is present at a position of at least 2θ = 20 ° to 25 °, and observation is performed after heating and cooling under the following heating / cooling condition 1 and heating / cooling condition 2 using DSC. A toner having a difference in glass transition temperature between the toners within 10 ° C. Temperature raising / lowering condition 1: The starting temperature is 20 ° C., the temperature is raised to 120 ° C. at 10 ° C./min, held at 120 ° C. for 10 minutes, lowered to 0 ° C. at 10 ° C./min, and 10 hours without holding time at 0 ° C. The temperature is raised to 150 ° C at a rate of ° C / min. Temperature rising / falling condition 2: The starting temperature is 20 ° C., the temperature is raised to 120 ° C. at 10 ° C./min, held at 120 ° C. for 10 minutes, lowered to 0 ° C. at 10 ° C./min, and 10 hours without holding time at 0 ° C. The temperature is raised to 45 ° C. at a rate of 45 ° C./min, held for 24 hours, again lowered to 0 ° C. at 10 ° C./min, and raised to 150 ° C. at 10 ° C./min without a holding time at 0 ° C. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11675285-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7013688-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019003131-A |
priorityDate | 2015-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 229.