http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016203447-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate | 2015-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebcc7ca00ed8e0fce0c2f84830e944fd |
publicationDate | 2016-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016203447-A |
titleOfInvention | Heat shrinkable film |
abstract | [PROBLEMS] To provide a heat-shrinkable film having excellent performance in both heat shrinkability, which is an indispensable characteristic as a shrink wrapping material, and gas barrier property, which is an important characteristic as a packaging material for fresh food. A heat-shrinkable film in which a gas barrier layer (II) is laminated on a plastic substrate (I), the plastic substrate (I) contains 0.1 to 70% by mass of a metal compound, and a gas barrier A heat-shrinkable film in which the layer (II) contains a polycarboxylic acid and satisfies the following characteristics (A) and (B) at the same time after being treated in hot water at 80 ° C. for 30 minutes. (A) Shrinkage is 15 to 40% (B) Oxygen permeability is 300ml / (m 2 · day · MPa) or less in an atmosphere with a temperature of 20 ° C and a relative humidity of 90% [Selection] None |