http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016195987-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C51-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C45-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C57-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-887 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C47-22 |
filingDate | 2015-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01d26a7987fee946ccdff45a48328842 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82493d033c2fc4b89cd33eedb4b66453 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2097f78d7be2c1c903ec9001fe45094 |
publicationDate | 2016-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016195987-A |
titleOfInvention | Composite oxide catalyst, method for producing acrolein and acrylic acid using the same |
abstract | As a composite oxide catalyst used for gas phase catalytic oxidation using an olefin as a raw material, the raw material is excellent in conversion rate even under conditions where the raw material contacts with the catalyst in a short time, and desired unsaturated aldehyde and unsaturated An object of the present invention is to provide a composite oxide catalyst having excellent strength that can maintain the selectivity of carboxylic acid at a high level, improve the yield, and can stably perform a gas phase catalytic oxidation reaction for a long period of time. A composite oxide catalyst for use in vapor phase catalytic oxidation of olefin, the composite oxide catalyst comprising an oxide of a plurality of specific elements, having a specific surface area of 5 m 2 / g to 25 m 2 / g, The pore volume occupied by pores having a pore volume of 0.20 ml / g to 0.50 ml / g and a pore diameter of 0.1 μm to 1.0 μm in the pore size distribution is the total pores 50% to 68% of the volume and a composite oxide catalyst in which the pore volume occupied by pores having a pore diameter diameter of less than 0.1 μm is 27% to 50% of the total pore volume. [Selection figure] None |
priorityDate | 2015-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |