http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016194688-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2016-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd2bd526fc8004c84afa9d76b7a6ccd9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_841006e0a39daf9f69e4a86a639d86fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_265d5050f96b54af391b2b5905b0fe7f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ea90ff2781cdd04af2ea766c6f70f9b |
publicationDate | 2016-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016194688-A |
titleOfInvention | Manufacturing method of toner binder |
abstract | PROBLEM TO BE SOLVED: Toner binder excellent in toner fluidity, heat-resistant storage stability, charge stability, pulverization property, image strength, folding resistance and document offset property while achieving both low-temperature fixability, glossiness and hot offset resistance. And a toner composition. SOLUTION: A melt mixture of a polyester resin (A) having a weight average molecular weight of 9,000 or more and 50,000 or less and a polyester resin (B) having a weight average molecular weight of 3,000 or more and less than 9,000 is added to a polyvalent resin. An isocyanate compound (D) was mixed and obtained by a production method characterized by comprising a step of obtaining a urethane-modified polyester resin (C) by reacting under conditions of 200 to 2,500 ppm of water in the system. A toner binder is used. [Selection figure] None |
priorityDate | 2015-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |