Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2310-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01Q60-32 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate |
2015-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e7e312c5aa27f4d68730dafed8295dd |
publicationDate |
2016-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2016128551-A |
titleOfInvention |
Rubber composition containing conjugated diene polymer and olefin polymer, and tire using the same |
abstract |
To provide a rubber composition for improving ozone resistance and a tire having improved ozone resistance. A rubber composition in which a domain formed from an olefin polymer is dispersed in a matrix composed of a nonpolar conjugated diene polymer, and after vulcanization, the matrix and the domain In a matrix comprising a rubber composition or a nonpolar conjugated diene polymer, wherein a chemical bond is present at the interface between them, and the dynamic compressive complex elastic modulus (E C * ) of the domain is 10 MPa or less In addition, a rubber composition in which domains formed from an olefin-based polymer are dispersed, and after vulcanization, chemical bonds exist at the interface between the matrix and the domains, and the average distance between the domains is It is a rubber composition characterized by being 2 μm or less. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019230699-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016128552-A |
priorityDate |
2015-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |