http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016110691-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 |
filingDate | 2014-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a97e7a907b504e8cb09ae42691a3076 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3880954a1ce0e911cbcb50c956eb9312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f8d23872fdd6e0d19c5f20aae6eb338 |
publicationDate | 2016-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016110691-A |
titleOfInvention | Method for manufacturing conductive substrate, and conductive substrate |
abstract | A method for manufacturing a conductive substrate capable of manufacturing a conductive substrate having excellent conductivity and adhesion is provided. A method for producing a conductive substrate having an organic-inorganic composite layer containing a siloxane skeleton and a porous metal layer in this order on one side of an insulating resin base material, comprising an alkoxysilyl group and a siloxane group. A metal particle dispersion containing a step of preparing a composition for an organic-inorganic composite layer containing an organic-inorganic composite material having at least one selected as a main component, a metal particle, a dispersant, and a solvent Preparing the organic-inorganic composite layer on the insulating resin substrate, forming the organic-inorganic composite layer, and forming the metal particle dispersion on the organic-inorganic composite layer. A method for producing a conductive substrate, comprising: a step of coating to form a coating film; and a step of forming a porous metal layer by firing the coating film by flash lamp annealing. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6169304-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11602922-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020524749-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018063768-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022044696-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111527450-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111527450-B |
priorityDate | 2014-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 197.