http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016108164-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8aa118fbfa85a6e0cc8c13a8afca19ab |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C8-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C8-24 |
filingDate | 2014-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4cf0363135327df7cb3c9817adec9274 |
publicationDate | 2016-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016108164-A |
titleOfInvention | Sealing glass and sealing material |
abstract | [PROBLEMS] To create a sealing glass and a sealing material using the same that soften and flow well in a low temperature region and have good weather resistance, and meet the recent environmental demands, while maintaining the environmental requirements of electronic components and display devices. Increase long-term reliability. SOLUTION: P5 + 0.1% or more, Sn2 + 1% or more, and anion%, F− + Cl−0.1 to 55%, and O2−45 to 99.9%. Glass to seal. [Selection figure] None |