http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016104896-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6038f17109882ad88e9ba8ea907ebb45 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2045-14868 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2705-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23F1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14311 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23F1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-02 |
filingDate | 2014-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81830fe1ddcd411be5262baf96bf8e95 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2357a51b4112689ed014deece054a9a9 |
publicationDate | 2016-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016104896-A |
titleOfInvention | Etching agent and replenisher thereof, method for roughening surface of magnesium component, and method for producing magnesium-resin composite |
abstract | The present invention provides an etching agent for a magnesium part capable of forming a roughened shape excellent in bondability with a resin on the surface of the magnesium part, and a surface roughening method for the magnesium part using the etching agent. An etchant of the present invention, one or more acids selected from the group consisting of inorganic acids and organic acids other than nitric; and the molecular structure N-OH or N-O - organic nitrogen compound containing It consists of the aqueous solution to contain. The concentration of the acid in the etching agent is 0.05 to 3% by weight, and the concentration of the organic nitrogen compound is 0.005 to 5% by weight. By bringing the etching agent into contact with the surface of the magnesium component, a fine roughened shape can be formed on the surface of the magnesium component even when the etching depth is large. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022230756-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023068133-A1 |
priorityDate | 2014-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 161.