http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016078322-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c46533e1bf04b5107543aa61c06dc5e5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D29-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G5-06 |
filingDate | 2014-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0bce118c661bfaefacd82c6e4636904b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68e85ae45cef98b99ffbcbe4c4d3ad56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd91352d8cd9798510ca2844dd654f14 |
publicationDate | 2016-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016078322-A |
titleOfInvention | Transmission belt and manufacturing method thereof |
abstract | A transmission belt is provided which is less likely to be disturbed. A method of manufacturing a transmission belt includes a step of molding and vulcanizing an endless tensile body layer 111 in which a core wire 112 extending in the belt length direction is embedded, and a molding of a rubber member 121A for a compressed rubber layer. And a step of performing vulcanization, and a step of bonding the vulcanized tensile body layer 111 and the vulcanized rubber member 121A for the compressed rubber layer with an adhesive rubber 122A interposed therebetween. The adhesive rubber 122A contains at least one of a thiazole vulcanization accelerator and an organic amine vulcanization accelerator. [Selection] Figure 9 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015122113-A1 |
priorityDate | 2014-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 87.