Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_86ff778280a8f314c5732fead5868411 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F41-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 |
filingDate |
2014-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d23d98bb6359ad8bc07093fb1ac8be22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_adce9875a9dde66fb07a688e6b8da51d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6516185e4c505ca565508f34154f863b |
publicationDate |
2016-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2016072519-A |
titleOfInvention |
Bond magnet and manufacturing method thereof |
abstract |
An object of the present invention is to improve the strength of a bonded magnet without deteriorating magnetic properties. A bonded magnet composed of a crystalline thermoplastic resin and magnetic powder is characterized in that the crystallization index represented by the following formula (A) is 85% or more. (A) Crystallization index = (calorific value due to crystallization−calorific value due to recrystallization) / calorific value due to crystallization) [selection] FIG. |