http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016069672-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C20-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10L3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C26-00 |
filingDate | 2014-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4bb20c0c030cea347d8656549b3e1a1d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_842d46a0071d10598ef9c53ac88afb5f |
publicationDate | 2016-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016069672-A |
titleOfInvention | Easy slip web manufacturing method |
abstract | The present invention provides a new production method capable of producing an easy-to-slip web having an easy-to-slip surface that can stably exhibit high slipperiness. Combusting a fuel composition to produce a flame, and applying a flame to a surface of a base web to obtain a slippery web having a slippery surface, the fuel composition comprising: A modifier raw material compound capable of generating a modifier capable of improving the slipperiness by adhering to the surface of the base web, and the coefficient of static friction after the tape peeling treatment of the slippery surface is 1.0. The manufacturing method of an easy-slip web which is the following. [Selection] Figure 1 |