Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_75249adb90a4cfa442d4751eea6ee07e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-24 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-03 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 |
filingDate |
2014-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61e88b24234e7e5bc9829426a9e8d15a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9d87df72909ed70f3360a8655ca2bf7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2536c62d0641cf773776c5db5c0db43f |
publicationDate |
2016-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2016068432-A |
titleOfInvention |
Painted body |
abstract |
An object of the present invention is to provide a coated body excellent in weather resistance, wear resistance and adhesion. A coated body comprising a substrate and a coating film disposed on the surface of the substrate, wherein the coating film is formed of a coating composition containing at least a fluorine resin and a resin other than the fluorine resin. When the ratio of fluorine atoms to the total mass of fluorine atoms and carbon atoms on the coating film surface is defined as the first fluorine concentration (% by mass), the first fluorine concentration is 30 to 50% by mass, The film thickness of the film is T (μm), and the ratio of fluorine atoms to the total mass of fluorine atoms and carbon atoms at the position of depth T / 2 (μm) from the coating film surface is the second fluorine concentration (mass%). The mass ratio (A / B) of the second fluorine concentration (A) to the first fluorine concentration (B) is 13/87 to 49/51. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6298198-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018104524-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018216297-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102416188-B1 |
priorityDate |
2014-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |