http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016064640-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 |
filingDate | 2015-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c94d47418e009467348c6e408d15fd6d |
publicationDate | 2016-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016064640-A |
titleOfInvention | Recording method |
abstract | There is provided a recording method capable of obtaining a recorded matter having good cohesiveness and printing durability and little recorded matter odor. A reaction liquid containing an aggregating agent capable of aggregating the components of a colored ink composition is adhered to a recording medium F at an adhesion amount of the aggregating agent of 100 to 1500 nmol / inch 2 to form a recording area S1. A reaction liquid deposition step to be formed, and a colored ink composition adhesion step in which a colored ink composition containing a colorant and a resin is deposited on the recording area S1 within 30 seconds from the deposition of the reaction liquid, thereby forming the recording area S2. And a recording method. [Selection] Figure 1 |
priorityDate | 2014-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |