http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016056226-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-05 |
filingDate | 2014-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_359313f9e421b0dda232f253ce7c2221 |
publicationDate | 2016-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016056226-A |
titleOfInvention | Silicone rubber composition and method for improving tear strength of cured silicone rubber |
abstract | (A) Organopolysiloxane containing an average of at least two alkenyl groups bonded to silicon atoms in one molecule: 100 parts by mass, (B) At least two hydrogen atoms bonded to silicon atoms in one molecule Organohydrogenpolysiloxane containing 0.5 to 20 parts by mass, (C) Fumed silica (dry silica) having a specific surface area of 50 to 400 m 2 / g by BET method: 10 to 40 parts by mass, (D) Wet silica having an average particle size of 2 μm or less: 2.5 to 3.5% by mass with respect to the total mass of component (A), component (B) and component (C), (E) addition reaction catalyst: containing catalyst amount Liquid addition curable silicone rubber composition. [Effect] According to the method of the present invention, the tear strength of silicone rubber obtained by heat-curing a liquid addition-curable silicone rubber composition can be stably improved. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018053237-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020184193-A1 |
priorityDate | 2014-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |