http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016041788-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 |
filingDate | 2014-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e90560b2e49feb165816948e59e2d0a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_abec9447448590f358c66730e2141777 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_511fa4f13dcd22a4195e610f31f379b9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d0dfce71305caeb4c0986c1ebf942d3 |
publicationDate | 2016-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016041788-A |
titleOfInvention | Polymer production method, polymer, and fluidity improver for aromatic polycarbonate resin |
abstract | An object of the present invention is to provide a fluidity improver for an aromatic polycarbonate resin that improves the melt fluidity during molding of an aromatic polycarbonate resin and improves the mechanical properties. . A vinyl monomer comprising a vinyl monomer (a1) having a specific structure of 0.5 to 99.5% by mass and another vinyl monomer (a2) of 0.5 to 99.5% by mass. A method for producing a polymer, wherein the mixture is radically polymerized in the presence of phenyl acetate. A fluidity improver for an aromatic polycarbonate resin, comprising a polymer obtained by the production method. [Selection figure] None |