http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016027983-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-22 |
filingDate | 2015-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ad2edf91d53d36a2919719862012739 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f444e82c339874ade1607adad5fc9b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e00aa1646ccdd2d3acddb43161dc74a5 |
publicationDate | 2016-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016027983-A |
titleOfInvention | Blow molded container, fuel container, and method for manufacturing blow molded container |
abstract | The object of the present invention is to suppress the occurrence of defects such as gelled blisters and streaks due to melt molding and coloring, to have excellent appearance and self-purge properties during production, to have quality such as sufficient strength, and to produce at low cost. A blow molded container, a fuel container, and a blow molded container manufacturing method are provided. A blow molded container comprising a first layer 1 mainly composed of EVOH obtained by saponifying a copolymer of ethylene and vinyl ester, wherein the EVOH uses a gel permeation chromatograph, The molecular weight measured after heat treatment at 220 ° C. for 50 hours in a nitrogen atmosphere satisfies the condition represented by the formula (1). (Ma−Mb) / Ma <0.45 (1) Ma: molecular weight in terms of PMMA at the maximum value of the peak measured by the differential refractive index detector Mb: wavelength 220 nm measured by the UV-visible absorbance detector Molecular weight in terms of PMMA at the maximum value of the absorption peak at [selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018003904-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109415133-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018003904-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109415133-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11279117-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019509380-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108805848-A |
priorityDate | 2014-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 260.