http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016026138-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8a9982b1666c54b5bf02d6c944891e4 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B17-064 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B17-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-091 |
filingDate | 2015-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0301faa183bb2510e3d0399d4bcaba39 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c15fc79eb2c33b1ee0e33f24d7e58a70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff485fe31d0a381a858fb434b1814325 |
publicationDate | 2016-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016026138-A |
titleOfInvention | Glass composition having high thermal and chemical stability and method for producing the same |
abstract | Disclosed is a glass for a liquid crystal display substrate having a high strain point and good dimensional stability and exhibiting chemical characteristics. SO2; 64.0-72.0, Al2O3; 9.0-16.0, B2O3; 1.0-5.0, MgO + La2O3 = 1.0-7. 5, CaO; 2.0-7.5, BaO; 1.0-7.0, SrO; 0.0-3.5, (1) Σ (MgO + CaO + SrO + BaO) / (Al 2 O 3) ≦ 1.50 Yes, (2) When the SrO content is not 0 mol%, the BaO / SrO ratio is 2.0 or more. (3) Other than SiO2, Al2O3, B2O3, MgO, CaO, BaO, SrO, La2O3 An alkali-free glass in which the amount of any oxide is 2.0 mol% or less and (4) the content of As2O3 and Sb2O3 is 0.005 mol% or less. [Selection figure] None |
priorityDate | 2006-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links