http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016015254-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fcc0b66123940d1b32783569ebfa2d45 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate | 2014-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da254f584902e665a58db316826defcb |
publicationDate | 2016-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016015254-A |
titleOfInvention | Method for filling container with binder composition for electricity storage device |
abstract | An object of the present invention is to provide a binder composition for an electricity storage device capable of producing an electrode having excellent storage stability and good adhesion and charge / discharge characteristics. The method for filling a container composition container for an electricity storage device according to the present invention comprises a binder composition for an electricity storage device containing a polymer (A) and a liquid medium (B), class 100,000. Hereinafter, the container is filled in an environment having a relative humidity of 30 to 90% RH. Moreover, the ratio of the volume of the space | gap part except the volume which the said binder composition for electrical storage devices accounts with respect to the internal volume of the said container is 1-25%. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018173839-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016079996-A1 |
priorityDate | 2014-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |