http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016006147-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 |
filingDate | 2014-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d6eb0d695f46bbf546427f74d3db15f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4bf8109758a6fdc65c123c052b34372 |
publicationDate | 2016-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2016006147-A |
titleOfInvention | Method for producing flexible polyurethane foam |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a flexible polyurethane foam having excellent tensile strength and cutting elongation and low residual TDA content. A polyol (composition) (P) and 2,4- and / or 2 containing an alkylene oxide adduct (A) of an active hydrogen-containing compound (h) and satisfying the following (1) and (2): , 6-Tolylene diisocyanate-containing organic polyisocyanate (B) is produced by reacting in the presence of a foaming agent (C), a urethanization catalyst (D), and a foam stabilizer (E). The (B) has an isocyanate index of 70 to 95, the polyurethane foam obtained has a total content of toluenediamine of 5 ppm or less, and a core density (kg / m 3 ) of 20 to 110. Method. (1) The primary hydroxyl group ratio of the terminal hydroxyl group of (P) is 10 to 80%. (2) The content of ethylene oxide units is 10% by weight or less based on the weight of (P). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018053169-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6157709-B1 |
priorityDate | 2013-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 135.